3PE Anti-corrosion Epoxy Powder Coating
Product Description:
This product utilizes linear novolac epoxy resin, designed and manufactured in accordance with GB/T 23257-2017. It shows high reactivity, strong coating adhesion, and high cross-linking density, resulting in a coating film with outstanding adhesion, chemical resistance, cathodic peeling resistance, and impact resistance.
Product features
1. Exhibits excellent adhesion to the substrate.
2. It possesses appropriate gelation time and interfacial properties, allowing easy fusion and bonding with the intermediate adhesive layer to form a unified structure upon curing.
3. Provides protection over a wide temperature range with long-lasting anti-corrosion effects.
4. The coating exhibits excellent resistance to high-temperature cathodic disbondment.
5. Large powder output area and high powder application rate.
6. Low melting temperature, high reaction activity, high curing completion rate, and excellent mechanical properties.
Technical parameter
(1) Performance Parameters of Powder Coatings
| No. | Experimental items | Qualitative index | Experimental Methodology |
| 1 | Appearance | Uniform color,free of lumps | visual |
| 2 | Color | As per customer requirements | |
| 3 | Density (g/cm³) | 1.4-1.6 | GB/T 4472 |
| 4 | Partical size distribution | The powder content on the 150 surface is ≤3.0The powder on the 250-mesh screen has a particle size ≤0.2 μm. | GB/T 6554 |
| 5 | Volatile matter content (%) | ≤0.6 | GB/T 6554 |
| 6 | Gelation time at 200°C (s) | ≥12 | GB/T 6554-1986 |
| 7 | Curing time at 200°C (min) | ≤3 | GB/T 23257-2017 Appendix A |
| 8 | Thermal performance | △H(J/g)≥45、Tg2≥95 | GB/T 23257-2017 Appendix B |
.
(II) Performance Parameters of the Solidified Powder Coating Film
| No. | Experimental items | Specifications | Experimental Methodology |
| 1 | Adhesion Strength (Level) | ≤2 | GB/T 23257-2017 Appendix C |
| 2 | 48-hour cathodic peeling resistance at 65°C (mm) | ≤8 | GB/T 23257-2017 Appendix D |
| 3 | 30-day cathodic peeling resistance at 65°C (mm) | ≤15 | GB/T 23257-2017 Appendix D |
| 4 | Bending resistance (-20°C, 2.5°) | No cracks | GB/T 23257-2017 Appendix E |
Implementation standard: GB/T 23257-2017
Application fields: Anti-corrosion coatings for various pipelines such as oil and gas transmission
Applicable technique: Electrostatic spraying