Anti-corrosion PE Powder Coating for RPE-D Pipeline
1、Product features
The anti-corrosion thermoplastic powder coating is specially designed for corrosion protection in pipelines used in power, cable, and construction applications. Leveraging the inherent corrosion-resistant properties of the base material combined with the incorporation of modifiers and functional additives during production, it forms cross-linked molecular structures that confer excellent mechanical performance and superior resistance to environmental stress cracking. This coating further enhances corrosion protection, providing effective protection and anti-aging performance for pipelines such as power cables.
2、 Product Technical Specifications and Applications
1.Technical specifications of anti-corrosion PE powder coating for pipelines
| 序号 | 检测项目 | 性能指标 | 执行标准 |
| 1 | 粉末粒度 | 60目筛上余物≤5% | GB/T6554-2003 |
| 2 | 流动性 | 上浮率≥20% | |
| 3 | 不挥发物含量 | >99.9% | GB/T6554-2003 |
| 4 | 熔融指数(g/10min) | 5-10 | GB/T3682 |
| No. | Test items | Performance index | Operative norm |
| 1 | Powder size | Remnants on the 60-mesh sieve ≤5% | GB/T6554-2003 |
| 2 | Flowability | The floating rate is ≥20% | |
| 3 | Non-volatile content | >99.9% | GB/T6554-2003 |
| 4 | Melt index (g/10 min) | 5-10 | GB/T3682 |
2.Technical Performance of PE Powder Coating Film for Pipeline Corrosion Protection
| No. | Test items | Performance index | Operative norm |
| 1 | Coating appearance | Uniform and smooth | |
| 2 | Peel strength N/cm | ≥40 | GB/T 2792: Liquidity |
| 3 | Flexual strength: 4° | 1 | |
| 4 | Impact strength | ≥21.6 | GB/T1040 |
| 5 | Low-temperature resistant catalytic property | ≤-65℃ | GB/T5470 |
| 6 | Electrical strength MV/m | 30 | GB/T1408.1 |
| 7 | Tensile strength MPA | ≥10 | GB/T1040 |
| 8 | Elongation at break % | ≥500 | GB/T1040 |
| 9 | Chemical-resistant (7 days)
10%HCL 10%NACL 10%NAOH |
≥80 ≥80 ≥80 |
GB/T23257-2017 |
| 10 | Heat-resistant aging percentage | ≤80 | GB/T3682 |
| Note : | 1. Resistance to chemical corrosion is measured by the retention rate of tensile strength and elongation at break after testing. | ||
| 2. The heat-resistant aging index is the deviation in fluid flow rate before and after the experiment. | |||
三、Coating Process
Surface pretreatment of steel pipes: Heating--Roll coating or Spraying--Cooling--Inspection--Packaging. Note: The heating temperature is 240°C ± 20°C, which can be adjusted according to the wall thickness of the steel pipe to achieve optimal coating film formation and corrosion protection efficacy.